Department of Applied Chemistry, Faculty of Textile Technology, University of Zagreb, 10000 Zagreb, Croatia.
Department of Material Testing, Faculty of Textile Technology, University of Zagreb, 10000 Zagreb, Croatia.
Molecules. 2022 May 18;27(10):3219. doi: 10.3390/molecules27103219.
Silver (Ag) and zinc (Zn) are very powerful antimicrobial metals. Therefore, in this research, a high-throughput, sensitive, and rapid method was developed for the determination of Ag and Zn in microcapsules using inductively coupled plasma mass spectrometry (ICP-MS). The sample preparation procedure employed simple microwave digestion of the microcapsules with 55.55% / HNO and 44.45% / HO. The method was applied to determine Ag and Zn in microcapsule samples of different sizes (120 and 450 μm) after their preparation with and without chitosan. Prepared microcapsules, after characterization, were bonded to a polymer carrier by sol-gel procedure and the materials were characterized by FTIR spectroscopy and high-resolution optical microscopy. Significant differences were found in Ag and Zn levels between microcapsules samples prepared with and without chitosan. The results have shown that samples with chitosan had up to 20% higher levels of Zn than Ag: 120 μm microcapsules contained 351.50 μg/g of Ag and 85.51 μg/g of Zn, respectively. In contrast, samples prepared without chitosan showed larger overall variability: In microcapsules with a diameter of 120 μm, the amounts of antimicrobial metals were 98.32 μg/g of Ag and 106.75 μg of Zn, respectively. Moreover, 450 μm microcapsules contained 190.98 μg/g of Ag and 121.35 μg/g of Zn. Those quantities are high enough for efficient antimicrobial activity of newly prepared microcapsules, enabling the application of microcapsules in different antimicrobial coatings.
银(Ag)和锌(Zn)是非常有效的抗菌金属。因此,在这项研究中,开发了一种高通量、灵敏、快速的方法,使用电感耦合等离子体质谱(ICP-MS)测定微胶囊中的Ag 和 Zn。样品制备程序采用简单的微波消解微胶囊,使用 55.55% / HNO 和 44.45% / HO。该方法应用于测定不同尺寸(120 和 450 μm)的微胶囊样品中 Ag 和 Zn,这些微胶囊在制备过程中使用和不使用壳聚糖。制备的微胶囊经过表征后,通过溶胶-凝胶程序与聚合物载体结合,并用傅里叶变换红外光谱和高分辨率光学显微镜对材料进行表征。在有和没有壳聚糖制备的微胶囊样品中,Ag 和 Zn 的水平存在显著差异。结果表明,含壳聚糖的样品中 Zn 的含量比 Ag 高 20%:120 μm 微胶囊分别含有 351.50 μg/g 的 Ag 和 85.51 μg/g 的 Zn。相比之下,没有壳聚糖制备的样品显示出更大的整体变异性:在直径为 120 μm 的微胶囊中,抗菌金属的量分别为 98.32 μg/g 的 Ag 和 106.75 μg 的 Zn。此外,450 μm 微胶囊含有 190.98 μg/g 的 Ag 和 121.35 μg/g 的 Zn。这些数量足以使新制备的微胶囊具有有效的抗菌活性,从而使微胶囊能够应用于不同的抗菌涂层中。