Jiang Yong-Hai, Xi Bei-Dou, Li Xiu-Jin, Wang Qi, Zhang Xiao-Xuan, Wei Zi-Min
College of Environmental Engineering, Beijing University of Chemical Technology, Beijing 100029, China.
Huan Jing Ke Xue. 2006 Nov;27(11):2288-92.
A kind of compound additive was studied and prepared in the paper, which associated with many functions. Using typical fly ash of Shanghai and Fuzhou, We studied the effect of the additive on evaporation rate, flowing temperature, fixed rate of heavy metals and its leaching characteristics in melting slag in the process of melting fly ash. The result showed that the flowing temperature and the evaporation rate of fly ash could be respectively reduced approximately 150 degrees C and 10% - 20% by adding 10% additive, and the fixed rate of heavy metals Cu and Pb increased 10% - 20%, especially Zn, which could increase 40%. The amount of leaching heavy metals in melting slag were both under corresponding standard limits using either national toxicity leaching methods or TCLP of EPA.
本文研究并制备了一种具有多种功能的复合添加剂。以上海和福州的典型粉煤灰为原料,研究了该添加剂对粉煤灰熔融过程中蒸发速率、流动温度、重金属固定率及其在熔渣中的浸出特性的影响。结果表明,添加10%的添加剂可使粉煤灰的流动温度和蒸发速率分别降低约150℃和10%-20%,重金属铜和铅的固定率提高10%-20%,特别是锌,可提高40%。无论是采用国家毒性浸出方法还是美国环保署的TCLP方法,熔渣中重金属的浸出量均低于相应的标准限值。